Standards AWS AWS B2.1-1/8-229: Standard welding procedure specification (SWPS) for gas tungsten arc welding followed by shielded metal arc welding of carbon steel (m-1/p-1/s-1, groups 1 or 2) to austenitic stainless steel (m-8/p-8/s-8, group 1), 1/8 through 1-1/2 inch
 AWS B2.1-1/8-229: Standard welding procedure specification (SWPS) for gas tungsten arc welding followed by shielded metal arc welding of carbon steel (m-1/p-1/s-1, groups 1 or 2) to austenitic stainless steel (m-8/p-8/s-8, group 1), 1/8 through 1-1/2 inch  pdf Download
Free
Price:  $  17.50 
Add to Cart

AWS B2.1-1/8-229: Standard welding procedure specification (SWPS) for gas tungsten arc welding followed by shielded metal arc welding of carbon steel (m-1/p-1/s-1, groups 1 or 2) to austenitic stainless steel (m-8/p-8/s-8, group 1), 1/8 through 1-1/2 inch pdf Download

File Size
244.45 KB
Year
2013
Number of Pages
27
Publisher
AWS
Samples
This standard contains the essential welding variables for welding carbon steel to austenitic stainless steel in the thickness range of 1/8 through 1-1/2 inch, using manual gas tungsten arc welding followed by shielded metal arc welding. It cites the base metals and operating conditions necessary to make the weldment, the filler metal specifications, and the allowable joint designs for groove and fillet welds. This SWPS was developed primarily for pipe applications.
Preview